A novel method for surface profilometry by holography is presented. We used a diode laser emitting at many wavelengths simultaneously as the light source and a Bi12TiO20 (BTO) crystal as the holographic medium in single exposure processes. The employ of multi-wavelength, large free spectral range (FSR) lasers leads to holographic images covered of interference fringes corresponding to the contour lines of the studied surface. In order to obtain the relief of the studied surface, the fringe analysis was performed by the phase stepping technique (PST) and the phase unwrapping was carried out by the Cellular-automata method. We analysed the relief of a tilted flat metallic bar and a tooth prosthesis.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

This study assessed the oral health of individuals 60 years or older in the city of Araraquara, Sao Paulo, Brazil, in 1998. Of the 194 people who participated in the study, 91 of them were institutionalized and had an average age of 73.6 years, and 103 were not institutionalized and had an average age of 69.3 years. The study participants were examined by a previously trained oral surgeon who determined the prevalence of the most common oral health problems. The results revealed a large number of edentulous individuals (72% of those institutionalized and 60% of the noninstitutionalized participants) and many persons with extracted teeth (93% and 90%, respectively), as well as a high frequency of periodontal pockets (57% and 75%, respectively) and of inadequate dentures (80% and 61%, respectively). Our results show reduced quality of life for a large proportion of these older individuals, and also indicate that public health services should pay greater attention to this population group.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Standardization of measurements for marginal fit of castings is critical. This study describes the fabrication of a device that allowed fixation of specimens on a Toolmakers microscope with identical conditions according to tri-dimensional positioning of specimens, measuring location, and seating force. The device also allows mapping of the marginal discrepancies on the entire marginal perimeter of the tooth preparation.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Utilization of contemporary post and core systems has facilitated the aesthetic restoration of endodontically treated teeth. Light transmission and biocompatibility have been enhanced by the introduction of metal-free post systems. The periodontal and endodontic status, root length, and histological structure of the devitalized teeth must be considered in order to achieve successful restoration following endodontic treatment. This article presents various restorative criteria for the aesthetic placement and buildup of post and core materials, as well as the preservation of maximum coronal and root structure.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Purpose: This investigation studied the effects of 3 surface treatments on the shear bond strength of a light-activated composite resin bonded to acrylic resin denture teeth. Materials and Methods: The occlusal surfaces of 30 acrylic resin denture teeth were ground flat with up to 400-grit silicon carbide paper. Three different surface treatments were evaluated: (1) the flat ground surfaces were primed with methyl methacrylate (MMA) monomer for 180 seconds; (2) light-cured adhesive resin was applied and light polymerized according to the manufacturer's instructions; and (3) treatment 1 followed by treatment 2. The composite resin was packed on the prepared surfaces using a split mold. The interface between tooth and composite was loaded at a cross-head speed of 0.5 mm/min until failure. Results: Analysis of variance indicated significant differences between the surface treatments. Results of mean comparisons using Tukey's test showed that significantly higher shear bond strengths were developed by bonding composite resin to the surfaces that were previously treated with MMA and then with the bonding agent when compared to the other treatments. Conclusion: Combined surface treatment of MMA monomer followed by application of light-cured adhesive resin provided the highest shear bond strength between composite resin and acrylic resin denture teeth.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Aim: The aim of this study was to evaluate the influence of ultrasound during the removal of posts cemented with either zinc phosphate cement, glass ionomer cement or resin cement. Methodology: Eighty-four single-rooted teeth were prepared and after cementation of cast posts, they were randomly divided into six groups of 14. Groups 1, 2 and 3 did not receive ultrasonic vibration, whilst groups 4, 5 and 6 received ultrasonic vibration for 10 min. The force necessary for post removal was determined using a universal testing machine. Results were statistically analysed using ANOVA and Tukey tests (5%). Results: The application of ultrasonic vibration reduced the retention provided by zinc phosphate and glass ionomer cements by 39% and 33%, respectively. Conclusions: A statistically significant reduction in the force necessary to remove posts cemented with zinc phosphate and glass ionomer cements occurred following application of ultrasound. The application of ultrasonic vibration did not influence the retention of cast posts cemented with resin cement.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Restorative dentistry has been increasingly concerned with preservation of the dental structure. For that reason, ultraconservative cavity preparations have been performed with air abrasion systems. The aim of this study was to present treatment options for the occlusal surface of first permanent molars with employment of the conventional method and the air abrasion system for accomplishment of the cavity preparation and a composite occlusal matrix for an accurate reproduction of the tooth surface.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The accuracy of impressions that transfer the relationship of the implant to the metal framework of the prosthesis continues to be a problem. This study was designed to evaluate the accuracy of the transfer process under variable conditions with regard to implant analog angulations, impression materials, and techniques. Replicas (n = 60) of a metal matrix (control) containing four implants at 90°, 80°, 75°, and 65° in relation to the horizontal surface were obtained by using three impression techniques: T1 - indirect technique with conical copings in closed trays; T2 - direct technique with square copings in open trays; and T3 - square copings splinted with autopolymerizing acrylic resin; and four elastomers: P-polysulfide; I-polyether; A-addition silicone; and Z-condensation silicone. The values of the implant analog annulations were assessed by a profilometer to the nearest 0.017°, then submitted to analysis of variance for comparisons at significance of 5% (P < .05). For implant analog at 90°, the material A associated with T2 and material Z with T3 behaved differently (P < .05) from all groups. At 80°, all materials behaved differently (P < .01) with T1. At 75°, when T1 was associated, materials P and A showed similar behavior, as well as materials I and Z; however, P and A were different from I and Z (P < .01). When T3 was associated, all experimental groups behaved differently among them (P < .01). At 65°, the materials P and Z behaved differently (P < .01) from the control group with T1, T2, and T3; the materials I and A behaved differently from the control group (P < .01) when T1 and T2, respectively, were associated. The more perpendicular the implant analog annulation is in relation to the horizontal surface, the more accurate the impression. The best materials were material I and A and the most satisfactory technique was technique 3.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Caries of primary incisors is a common problem in paediatric dentistry in some countries. The restoration of primary incisors which have been severely damaged by early childhood caries or trauma is also a difficult challenge for clinicians. This case report describes an indirect technique for the restoration of primary anterior teeth using composite resin reinforced with a fibreglass post. Over a one-year period, the crowns have demonstrated good retention and aesthetic results. The restorations were provided in two short chair-side sections, with satisfactory patient cooperation. © 2005 BSPD and IAPD.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

The purpose of this study was to histomorphometrically evaluate the bone-to-implant contact and bone area around a titanium implant retrieved from a human lower jaw. A screw-shaped titanium implant (sandblasted and acid-etched surface) was removed from a 68-year-old male after having been in function for 40 months because of a fracture of the abutment screw. Following the implant removal, an undecalcified section was obtained. The histomorphometric analysis showed a rate of 75.40% of bone-to-implant contact and 89.30% of bone area filling within the limits of the implant threads. The surrounding bone healed in a well-organized pattern and could not be differentiated from the anginal alveolus. The histologic evidence showed a high degree of osseointegration in a threaded, sandblasted, and acid-etched implant retrieved from a human lower jaw after functional loading for 40 months. Copyright © 2005 by Lippincott Williams & Wilkins.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Purpose: To determine whether intercommissural width is a reliable guide for the selection of maxillary denture teeth width. Materials and Methods: Casts were made of 160 subjects from 4 different racial groups. Locations of intercommissural width landmarks (the corners of the mouth) were made on the subjects and transferred to the casts. The distances between the corners of the mouth and the distal of the canines were measured on the casts and compared. Results: A weak correlation was found between the distal of the canines and the distance between the corners of the mouth in the 4 racial groups. Conclusion: The use of the corners of the mouth for the selection of artificial teeth is generally inaccurate.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Purpose: Fiber-reinforced composite (FRC) posts can be air-abraded to obtain good attachment to the resin cement. This study tested the effect of silica coating on the flexural strength of carbon, opaque, and translucent quartz FRC posts. Materials and Methods: Six experimental groups of FRC posts (n = 10 per group) were tested, either as received from the manufacturer or after chairside silica coating (30-μm CoJet-Sand). Results: There was no significant difference in the flexural strength of nonconditioned (504 to 525 MPa) and silica-coated (514 to 565 MPa) specimens (P > .05) (analysis of variance). The type of post did have a significant effect on flexural strength (P < .05). Conclusion: Chairside silica coating did not affect the flexural strength of both carbon and quartz FRC posts.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

This study evaluated the effect of three surface conditioning methods on the microtensile bond strength of resin cement to a glass-infiltrated zirconia-reinforced alumina-based core ceramic. Thirty blocks (5×5×4 mm) of In-Ceram Zirconia ceramics (In-Ceram Zirconia-INC-ZR, VITA) were fabricated according to the manufacturer's instructions and duplicated in resin composite. The specimens were polished and assigned to one of the following three treatment conditions (n=10): (1) Airborne particle abrasion with 110 μm Al2O3 particles + silanization, (2) Silica coating with 110 μm SiOx particles (Rocatec Pre and Plus, 3M ESPE) + silanization, (3) Silica coating with 30 μm SiOx particles (CoJet, 3M ESPE) + silanization. The ceramic-composite blocks were cemented with the resin cement (Panavia F) and stored at 37 °C in distilled water for 7 days prior to bond tests. The blocks were cut under coolant water to produce bar specimens with a bonding area of approximately 0.6 mm2. The bond strength tests were performed in a universal testing machine (cross-head speed: 1 mm/min). The mean bond strengths of the specimens of each block were statistically analyzed using ANOVA and Tukey's test (α≤0.05). Silica coating with silanization either using 110 μm SiOx or 30 μm SiOx particles increased the bond strength of the resin cement (24.6±2.7 MPa and 26.7±2.4 MPa, respectively) to the zirconia-based ceramic significantly compared to that of airborne particle abrasion with 110-μm Al2O3 (20.5±3.8 MPa) (ANOVA, P<0.05). Conditioning the INC-ZR ceramic surfaces with silica coating and silanization using either chairside or laboratory devices provided higher bond strengths of the resin cement than with airborne particle abrasion using 110 μm Al2O3. © 2005 Academy of Dental Materials. Published by Elsevier Ltd. All rights reserved.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Purpose: To evaluate the fatigue resistance of the bond between dentin and glass-infiltrated alumina ceramic, using different luting protocols. Materials and Methods: The null hypothesis is that the fatigue resistance varies with the luting strategy. Forty blocks of In-Ceram Alumina were prepared, and one surface of each block was abraded with 110-μm aluminum oxide particles. Then, the blocks were luted to flat dentin surfaces of 40 human third molars, using 4 different luting strategies (luting system [LS]/ceramic surface conditioning [CSC]) (n=10): (G1) [LS] RelyX-Unicem/[CSC] airborne abrasion with 110-μm Al2O3 particles; (G2) [LS] One-Step + Duo-Link (bis-GMA-based resin)/[CSC] etching with 4% hydrofluoric acid + silane agent; (G3) [LS] ED-Primer + Panavia F (MDP-based resin)/[CSC] Al2O 3; (G4) [LS] Scotchbond1+RelyX-ARC (bis-GMA-based resin)/[CSC] chairside tribochemical silica coating (air abrasion with 30-μm SiO x particles + silane). After 24 h of water storage at 37°C, the specimens were subjected to 106 fatigue cycles in shear with a sinusoidal load (0 to 21 N, 8 Hz frequency, 37°C water). A fatigue survivor score was given, considering the number of the fatigue cycles until fracture. The failure modes of failed specimens were observed in a SEM. Results: G3 (score = 5.9, 1 failure) and G4 (score = 6, no failures) were statistically similar (p = 0.33) and had significantly higher fatigue resistance than G1 (score = 3.9, 5 failures) and G2 (score = 3.7, 6 failures) (p < 0.03). SEM analysis of fractured specimens of G1 and G2 showed that almost all the failures were between ceramic and cement. Conclusion: The MDP-based resin cement + sandblasting with Al2O3 particles (G3) and bis-GMA-based resin cement + tribochemical silica coating (G4), both using the respective dentin bonding systems, were the best luting protocols for the alumina ceramic. The null hypothesis was confirmed.

Relevância:

60.00% 60.00%

Publicador:

Resumo:

Purpose: The aim of this study was to evaluate the effect of two surface conditioning methods on the microtensile bond strength of a resin cement to three high-strength core ceramics: high alumina-based (In-Ceram Alumina, Procera AllCeram) and zirconia-reinforced alumina-based (In-Ceram Zirconia) ceramics. Materials and Methods: Ten blocks (5 ×6 × 8 mm) of In-Ceram Alumina (AL), In-Ceram Zirconia (ZR), and Procera (PR) ceramics were fabricated according to each manufacturer's instructions and duplicated in composite. The specimens were assigned to one of the two following treatment conditions: (1) airborne particle abrasion with 110-μm Al2O3 particles + silanization, (2) silica coating with 30 μm SiOx particles (CoJet, 3M ESPE) + silanization. Each ceramic block was duplicated in composite resin (W3D-Master, Wilcos, Petrópolis, RJ, Brazil) using a mold made out of silicon impression material. Composite resin layers were incrementally condensed into the mold to fill up the mold and each layer was light polymerized for 40 s. The composite blocks were bonded to the surface-conditioned ceramic blocks using a resin cement system (Panavia F, Kuraray, Okayama, Japan). One composite resin block was fabricated for each ceramic block. The ceramic-composite was stored at 37°C in distilled water for 7 days prior to bond tests. The blocks were cut under water cooling to produce bar specimens (n = 30) with a bonding area of approximately 0.6 mm2. The bond strength tests were performed in a universal testing machine (crosshead speed: 1 mm/min). Bond strength values were statistically analyzed using two-way ANOVA and Tukey's test (≤ 0.05). Results: Silica coating with silanization increased the bond strength significantly for all three high-strength ceramics (18.5 to 31.2 MPa) compared to that of airborne particle abrasion with 110-μm Al2O3 (12.7-17.3 MPa) (ANOVA, p < 0.05). PR exhibited the lowest bond strengths after both Al2O3 and silica coating (12.7 and 18.5 MPa, respectively). Conclusion: Conditioning the high-strength ceramic surfaces with silica coating and silanization provided higher bond strengths of the resin cement than with airborne particle abrasion with 110-μm Al2O3 and silanization.